DIN 1.2766 Tool steels
Data updates
This material has 241 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
DIN 1.2766 Chemical Composition
Edelstahlwerk W. Ossenberg & Cie. GmbH, Product Data Sheets,
Looking for full material performance data?
Free registration required • Instant access
DIN 1.2766 Physical Properties
Temperature
This material has 241 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
DIN 1.2766 Heat Treatments
- Operation of hardening - 820-850°C; Hardness, Brinell, HB 30 < 260; Hardness HRc 1770 MPa, Working resistance 1180-1620 MPa; Hot working 1050-850°C; Soft annealing 620-680°C; Temper 350-600°C
DIN 1.2766 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
DIN 1.2766 International Equivalent Materials
Showing 15 of 113 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 113 international equivalents?
See all 113 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 113Cross References
- 8Composition
- 1Mechanical Properties
- 3Physical Properties
- 3Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 113Total Suppliers