DIN 1.0757 Structural and constructional steels
Data updates
This material has 426 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
DIN 1.0757 Chemical Composition
EN 10087: 1998 / Free-cutting steels - Technical delivery conditions for semi-finished products, hot-rolled bars and rods
Looking for full material performance data?
Free registration required • Instant access
DIN 1.0757 Physical Properties
Temperature
This material has 426 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
DIN 1.0757 Heat Treatments
- Operation of hardening - Oil 830-860; Temper 540-680/min. 1 h; Operation of hardening - Water 820-850
- Quenching: 840-870°C (0.5h minimum), water or oil cooling;
Tempering: 540-680°C (1h minimum).
DIN 1.0757 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
DIN 1.0757 International Equivalent Materials
Showing 15 of 104 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 104 international equivalents?
See all 104 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 104Cross References
- 31Composition
- 227Mechanical Properties
- 3Physical Properties
- 3Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- 2Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 56Total Suppliers