1.0335 (Germany / DIN) Material Properties

Other designations: ,
Material group: Ferrous Alloys / Structural and constructional steels
Country/Standard: Germany / DIN

Data updates

Latest Update: 2025-02
Total number of updates: 2
Update History:
2015-06

Mechanical Properties


Temperature

0 - 30°C
PROPERTY / VALUE
Yield Strength, Rp0.2 170 — 330 MPa view details
Tensile Strength ≤ 410 MPa view details
Elongation, A 27 % view details
Yield Strength, Rp0.2 24.7 — 47.9 ksi view details
Tensile Strength ≤ 59.5 ksi view details
Elongation, A 27 % view details

Physical Properties


Temperature

0 - 30°C
PROPERTY / VALUE
Modulus of Elasticity 190 — 210 GPa view details
Density 7.67 — 7.86 kg/dm³ view details
Poisson Coefficient 0.27 — 0.3 view details
Modulus of Elasticity 27.6 E+03 — 30.5 E+03 ksi view details
Density 0.277 — 0.284 lb/in³ view details
Poisson Coefficient 0.27 — 0.3 view details

Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
≤ 0.08
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Mn
VALUE
≤ 0.40
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
P
VALUE
≤ 0.030
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7704-34-9

EN 10111: 2008 / Continuously hot-rolled low carbon steel sheet and strip for cold forming - Technical delivery conditions

Heat Treatments

Since direct data is not available in the original source, register for a free trial to explore similar or equivalent materials having these properties.

Register Now