CSN 42 2736 Cast steels
Material group:
Ferrous Alloys / Cast steels
Country / Standard:
Czech Republic / CSN
Data updates
Latest Update: 2015-07
Total number of updates: 1
Update History
This material has 42 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
View Complete Material Data ›
Free registration required • Instant access
Free registration required • Instant access
CSN 42 2736 Chemical Composition
CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
0.6000 – 0.7500
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
1.8000 – 2.2000
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Mn
VALUE
0.8000 – 1.2000
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
P
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
P+S
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
CRITERIA
S
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7440-21-3
CSN 42 2736: 1980 / Steel 42 2736 for castings Mn-Cr
Looking for full material performance data?
View Complete Material Data ›
Free registration required • Instant access
Free registration required • Instant access
CSN 42 2736 Physical Properties
Temperature
Modulus of Elasticity
212.5
GPa
Unlock full details
Full data available with free access
View Complete Material Data
Thermal Conductivity
Unlock full details
Full data available with free access
View Complete Material Data
Density
Unlock full details
Full data available with free access
View Complete Material Data
Heat Capacity
Unlock full details
Full data available with free access
View Complete Material Data
This material has 42 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
View Complete Material Data ›
Free registration required • Instant access
Free registration required • Instant access
CSN 42 2736 Heat Treatments
- Normalizing at 820 to 860°C, cooling in air; Tempering at 630 to 680°C, cooling in furnace, air; Annealing to lower tension at 600 to 650°C cooling in furnace, air. Temperature annealing for stress relief should be about 20-30°C lower than the actual temperature tempering;
CSN 42 2736 Mechanical Properties
Temperature
Tensile Strength
800 — 1000
MPa
Unlock full details
Full data available with free access
View Complete Material Data
Brinell Hardness (HB)
235 — 295
Unlock full details
Full data available with free access
View Complete Material Data
Elongation, A
≥ 4
%
Unlock full details
Full data available with free access
View Complete Material Data
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
View Complete Material Data ›
Book A Demo
Free registration required • Instant access
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 2Cross References
- 7Composition
- 3Mechanical Properties
- 29Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- -Total Suppliers