CSN 19 642 Tool steels
Material group:
Ferrous Alloys / Tool steels
Country / Standard:
Czech Republic / CSN
Data updates
Latest Update: -
Total number of updates: 0
This material has 14 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
View Complete Material Data ›
Free registration required • Instant access
Free registration required • Instant access
CSN 19 642 Chemical Composition
CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
0.3000 – 0.4000
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
0.7000 – 1.1000
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Mn
VALUE
0.4000 – 0.7000
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Mo
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7439-98-7
CRITERIA
Ni
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7440-02-0
CRITERIA
P
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7440-21-3
CSN 41 9642 / Ni-Cr-Mo tool steel 19 642
Looking for full material performance data?
View Complete Material Data ›
Free registration required • Instant access
Free registration required • Instant access
CSN 19 642 Physical Properties
Temperature
Modulus of Elasticity
190 — 210
GPa
Unlock full details
Full data available with free access
View Complete Material Data
Density
7.72 — 8
kg/dm³
Unlock full details
Full data available with free access
View Complete Material Data
Poisson Coefficient
0.27 — 0.3
Unlock full details
Full data available with free access
View Complete Material Data
This material has 14 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
View Complete Material Data ›
Free registration required • Instant access
Free registration required • Instant access
CSN 19 642 Heat Treatments
- Hot forming: 1050-800 ºC; Annealing: 610-630 ºC 4-8h; Hardening in oil: 820-850 ºC; Tempering: according to requirements approx. 280 ºC or stronger 540 ºC;
CSN 19 642 Mechanical Properties
Temperature
Tensile Strength
≥ 883
MPa
Unlock full details
Full data available with free access
View Complete Material Data
Brinell Hardness (HB)
≤ 260
Unlock full details
Full data available with free access
View Complete Material Data
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
View Complete Material Data ›
Book A Demo
Free registration required • Instant access
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- -Cross References
- 8Composition
- 2Mechanical Properties
- 3Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- -Total Suppliers