CSN 19 614 Tool steels

Material group: Ferrous Alloys / Tool steels
Country / Standard: Czech Republic / CSN

Data updates

Latest Update: -
Total number of updates: 0

This material has 18 properties — only a subset is shown here.

Unlock full material properties, including detailed values across temperatures and conditions.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

CSN 19 614 Chemical Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
0.5000 – 0.6000
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
0.6000 – 0.9000
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Mn
VALUE
0.4000 – 0.7000
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Ni
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7440-02-0
CRITERIA
P
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7440-21-3
CRITERIA
V
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7440-62-2

CSN 41 9614 / Ni-Cr-V tool steel 19 614

Looking for full material performance data?

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

CSN 19 614 Physical Properties


Temperature

PROPERTY / VALUE
Modulus of Elasticity
190 — 210 GPa
Unlock full details
Full data available with free access View Complete Material Data
Density
7.72 — 8 kg/dm³
Unlock full details
Full data available with free access View Complete Material Data
Poisson Coefficient
0.27 — 0.3
Unlock full details
Full data available with free access View Complete Material Data

This material has 18 properties — only a subset is shown here.

Unlock detailed physical values across temperatures and conditions.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

CSN 19 614 Heat Treatments


  • Hot forming: 1050-800 ºC; Annealing: 740-760 ºC 2-4h; Hardening in oil: 780-820 ºC; Tempering: according to requirements approx. 180-250 ºC or stronger;

CSN 19 614 Mechanical Properties


Temperature

PROPERTY / VALUE
Tensile Strength
≥ 735 MPa
Unlock full details
Full data available with free access View Complete Material Data
Brinell Hardness (HB)
≤ 610
Unlock full details
Full data available with free access View Complete Material Data

Need complete mechanical properties to make the right choice?

Get complete data on strength, hardness, fatigue, and more.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

Book A Demo

Optimize material selection for your application - Book A Demo

  • -Cross References

  • 8Composition
  • 6Mechanical Properties
  • 3Physical Properties
  • 1Heat Treatment
  • -Metallography
  • -Machinability

  • -Stress-Strain
  • -Formability
  • -Fatigue
  • -Fracture
  • -Creep

  • -Joints
  • -Coatings
  • -Dimensions
  • -Tribology

  • -Corrosion
  • -Ageing
  • -Weatherability
  • -Irradiation

  • -Total Suppliers