CSN 17 252 Stainless steels
Material group:
Ferrous Alloys / Stainless steels
Country / Standard:
Czech Republic / CSN
Data updates
Latest Update: 2018-06
Total number of updates: 1
Update History
This material has 43 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
View Complete Material Data ›
Free registration required • Instant access
Free registration required • Instant access
CSN 17 252 Chemical Composition
CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
≤ 0.08
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
19.0 – 22.0
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Mn
VALUE
≤ 1.50
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Mo
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7439-98-7
CRITERIA
Ni
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7440-02-0
CRITERIA
P
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7440-21-3
CRITERIA
Ti
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7440-32-6
CSN 41 7252: 1985 / Chromium-Nickel-Molybdenum steel 17 252
Looking for full material performance data?
View Complete Material Data ›
Free registration required • Instant access
Free registration required • Instant access
CSN 17 252 Physical Properties
Temperature
Modulus of Elasticity
190 — 215
GPa
Unlock full details
Full data available with free access
View Complete Material Data
Electrical Resistivity
1.1
Ω∙mm²/m
Unlock full details
Full data available with free access
View Complete Material Data
Density
Unlock full details
Full data available with free access
View Complete Material Data
Electrical Conductivity
Unlock full details
Full data available with free access
View Complete Material Data
Poisson Coefficient
val1
Full data available with free access
View Complete Material Data
Unlock full details
Full data available with free access
View Complete Material Data
Thermal Conductivity
16.7
W/(m∙°C)
Unlock full details
Full data available with free access
View Complete Material Data
This material has 43 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
View Complete Material Data ›
Free registration required • Instant access
Free registration required • Instant access
CSN 17 252 Heat Treatments
- Hot forming at 1150 - 900°C;
Annealing at 1050 to 1100°C, warm and cool in the water;
Stabilization annealing at 850 to 900°C, 2 to 4 hours.
CSN 17 252 Mechanical Properties
Temperature
Tensile Strength
≥ 590
MPa
Unlock full details
Full data available with free access
View Complete Material Data
Elongation, A
≥ 32
%
Unlock full details
Full data available with free access
View Complete Material Data
Reduction of Area
Unlock full details
Full data available with free access
View Complete Material Data
Yield Strength, Rp0.2
≥ 225
MPa
Unlock full details
Full data available with free access
View Complete Material Data
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
View Complete Material Data ›
Book A Demo
Free registration required • Instant access
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- -Cross References
- 9Composition
- 15Mechanical Properties
- 15Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- 3Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- -Total Suppliers