CSN 14 160 Structural and constructional steels
Material group:
Ferrous Alloys / Structural and constructional steels
Country / Standard:
Czech Republic / CSN
Indicative price:
Data updates
Latest Update: 2016-08
Total number of updates: 1
Update History
This material has 26 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
View Complete Material Data ›
Free registration required • Instant access
Free registration required • Instant access
CSN 14 160 Chemical Composition
CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
0.5000 – 0.6000
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
0.3000 – 0.5000
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Cu
VALUE
≤ 0.3000
UNIT
%
CAS NUMBER
7440-50-8
CRITERIA
Mn
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Ni
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7440-02-0
CRITERIA
P
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7440-21-3
CSN 41 4160: 1976 / Manganese-Chromium steel 14 160
Looking for full material performance data?
View Complete Material Data ›
Free registration required • Instant access
Free registration required • Instant access
CSN 14 160 Physical Properties
Temperature
Modulus of Elasticity
190 — 210
GPa
Unlock full details
Full data available with free access
View Complete Material Data
Density
7.67 — 7.86
kg/dm³
Unlock full details
Full data available with free access
View Complete Material Data
Poisson Coefficient
0.27 — 0.3
Unlock full details
Full data available with free access
View Complete Material Data
This material has 26 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
View Complete Material Data ›
Free registration required • Instant access
Free registration required • Instant access
CSN 14 160 Heat Treatments
- Rolling, bending, forging at 1100 to 800°C, cooling slowly.
Normalizing at 820 to 840°C, cooling slowly in air.
Hardening at 800 to 820°C, cooling slowly in oil.
Tempering at 400 to 550°C, cooling in air.
Soft annealing at 700 to 740°C, 4h, slowly cooling in the furnace.
CSN 14 160 Mechanical Properties
Temperature
Tensile Strength
≥ 785
MPa
Unlock full details
Full data available with free access
View Complete Material Data
Brinell Hardness (HB)
≥ 211
Unlock full details
Full data available with free access
View Complete Material Data
Elongation, A
≥ 8
%
Unlock full details
Full data available with free access
View Complete Material Data
Reduction of Area
Unlock full details
Full data available with free access
View Complete Material Data
Vickers Hardness (HV)
val1
Full data available with free access
View Complete Material Data
Unlock full details
Full data available with free access
View Complete Material Data
Yield Strength, Rp0.2
Unlock full details
Full data available with free access
View Complete Material Data
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
View Complete Material Data ›
Book A Demo
Free registration required • Instant access
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- -Cross References
- 8Composition
- 10Mechanical Properties
- 4Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- 1Stress-Strain
- 2Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- -Total Suppliers