En38 (United Kingdom / B.S.) Material Properties

Material group: Ferrous Alloys / Structural and constructional steels
Country/Standard: United Kingdom / B.S.

Data updates

Latest Update: -
Total number of updates: 0
Update History:
-

Mechanical Properties


Temperature

0 - 30°C
PROPERTY / VALUE
Tensile Strength 1004 MPa view details
Elongation, A 13 % view details
Tensile Strength 145.6 ksi view details
Elongation, A 13 % view details

Physical Properties


Temperature

0 - 30°C
PROPERTY / VALUE
Modulus of Elasticity 190 — 210 GPa view details
Density 7.67 — 7.86 kg/dm³ view details
Poisson Coefficient 0.27 — 0.3 view details
Modulus of Elasticity 27.6 E+03 — 30.5 E+03 ksi view details
Density 0.277 — 0.284 lb/in³ view details
Poisson Coefficient 0.27 — 0.3 view details

Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
≤ 0.16
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
≤ 0.3
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Mn
VALUE
≤ 0.60
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Mo
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7439-98-7
CRITERIA
Ni
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-02-0
CRITERIA
P
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-21-3

Wrought steels for mechanical and allied engineering purposes, BS 970

Heat Treatments