B.S. T 75 Stainless steels
Data updates
This material has 25 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
B.S. T 75 Chemical Composition
BS T 75: 1972 / Specification for low carbon 17/12 chromium-nickel-molybdenum corrosion-resisting steel tube (500 N/mm2)
Looking for full material performance data?
Free registration required • Instant access
B.S. T 75 Physical Properties
Temperature
This material has 25 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
B.S. T 75 Heat Treatments
- Softening shall be carried out by heating at a temperature between 1000°C and 1100°C and cooling in a suitable manner.
B.S. T 75 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
B.S. T 75 International Equivalent Materials
Showing 1 of 3 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 3 international equivalents?
See all 3 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 3Cross References
- 8Composition
- 10Mechanical Properties
- 3Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- -Total Suppliers