Article Corrosion of Carbon Steel 7 min read • October 2001 • Sélection des matériaux › Matériaux résistants à la corrosion • Dernière révision technique : 2026 Abstract This comprehensive article examines the corrosion behavior of carbon steel, the most widely used engineering material globally. It explores various types of corrosion affecting carbon steel, including atmospheric, aqueous, and soil corrosion, while analyzing the impact of environmental factors and alloying elements on corrosion resistance. The study highlights protective measures and factors influencing corrosion rates across different applications, from marine environments to industrial settings, providing valuable insights for engineers and materials scientists working with carbon steel structures and equipment. Introduction to Carbon Steel Corrosion Carbon steel, accounting for approximately 85% of annual steel production worldwide, remains the backbone of industrial infrastructure despite its limited corrosion resistance. Its applications span marine installations, nuclear and fossil fuel power plants, transportation systems, chemical processing facilities, petroleum production, pipelines, mining operations, construction projects, and metal-processing equipment. The economic impact of metallic corrosion reaches hundreds of millions of dollars annually. As carbon steels constitute the largest class of alloys in use, both in tonnage and cost, their corrosion presents a significant industrial challenge, spawning entire industries dedicated to developing protective systems. Composition and Corrosion Resistance Carbon steels typically contain less than 2% by weight of alloying elements. While these limited additions generally don't dramatically improve corrosion resistance, weathering steels represent an exception. Small additions of copper, chromium, nickel, and phosphorus can significantly reduce corrosion rates in specific environments. Types of Corrosion Atmospheric Corrosion Atmospheric environments are classified as rural, industrial, or marine. Corrosion rates vary significantly based on factors including: Average yearly temperature Rainfall patterns Mean temperature Presence of acid rain Relative humidity Atmospheric pollutants The corrosion process requires both oxygen and water, with even a thin adsorbed water film sufficient to initiate the process. Exposure time to moisture, particularly influenced by relative humidity, plays a crucial role in determining corrosion rates. Aqueous Corrosion Water exposure presents varying corrosion challenges depending on: Temperature Flow rate pH levels Solution composition Choisir des matériaux résistants à la corrosion Comparez les matériaux résistants à la corrosion à l'aide de données référencées concernant leur résistance aux conditions environnementales, leur durabilité et leurs performances. Comparer les matériaux Faites une visite guidée › In acidic conditions, hydrogen evolution prevents protective film formation, while alkaline solutions promote protective films that reduce corrosion rates. Seawater corrosion, while similar in overall rate to freshwater, tends to cause more localized pitting due to higher electrical conductivity. Table 1. Comparison of results under different type of exposure Effects of alloy selection, chemical composition and alloy additions Sea air Freshwater Alternately wet with seawater or Spray and dry Continuously wet with seawater Ferrous alloys Pockmarked Vermiform on cleaned bars Pitting, particularly on bars with scale Pitting, particularly on bars with scale Wrought iron versus carbon steel Steel superior to wrought and ingot irons Iron and steel equal in low-moor areas Low-moor iron superior to carbon steel Low-moor iron superior to carbon steel Sulfur and phosphorus content Best results when S and P are low Best results when S and P are low Best results when S and P are low Apparently little influence Addition of copper Beneficial: Effect increasing with copper content Beneficial: 0.635% Cu almost as good as 2.185% Cu Beneficial: 0.635% and 2.185% Cu much the same 0.635% Cu slightly beneficial: 2.185% Cu somewhat less so Addition of nickel 3.75% Ni superior even to 2% Cu; 36% Ni almost perfect after 15-year exposure 3.75%Ni superior even to 2%Cu; 36%Ni excellent resistance 3.75%Ni beneficial usually more so than Cu: 36%Ni the best metal in the set 3.75% Ni slightly beneficial and slightly superior to Cu: 36% Ni the best metal in the set Addition of 13.5% Cr Excellent resistance to corrosion: cold blast metal perfect after 15-year exposure: equal to 36% Ni steel Excellent resistance to corrosion: equal to 36% Ni steel Subject to severe localized corrosion that virtually destroys the metal Subject to severe localized corrosion that virtually destroys the metal Behavior of cast irons Excellent resistance to corrosion: cold blast metal superior to hot: no graphitic corrosion Undergoes graphitic corrosion Undergoes graphitic corrosion Undergoes graphitic corrosion Soil Corrosion Soil corrosion severity depends primarily on: Soil composition Moisture content Oxygen availability Electrical conductivity Acidity levels Dissolved salt content The corrosion rate can be expressed mathematically as Z = a·tm, where Z represents weight loss or maximum pit depth, t is exposure time, and a and m are situation-specific constants.