AA Alclad 2024 Aluminiumlegierungen
Datenaktualisierungen
Dieser Werkstoff verfügt über 712 Eigenschaften – hier wird nur ein Teil davon angezeigt.
Erhalten Sie Zugriff auf alle Werkstoffeigenschaften, einschließlich detaillierter Werte für verschiedene Temperaturen und Zustände.
Kostenlose Registrierung erforderlich • Sofortiger Zugriff
AA Alclad 2024 Physikalische Eigenschaften
Temperatur
Dieser Werkstoff verfügt über 712 Eigenschaften – hier wird nur ein Teil davon angezeigt.
Erhalten Sie detaillierte physikalische Werte für verschiedene Temperaturen und Bedingungen.
Kostenlose Registrierung erforderlich • Sofortiger Zugriff
AA Alclad 2024 Wärmebehandlung
- The times and temperatures are typical for various forms, sizes and methods of manufacture and may not exactly describe the optimum treatment for a specific item.
The nominal temperatures at which metal is heated (applies both for solution and precipitation heat treatment) should be attained as rapidly as possible and maintained ± 5°C of nominal during the time at temperature.
The time at precipitation heat treatment temperature will depend on time required for load to reach temperature. The times shown are based on rapid heating, with soaking time measured from the time the load reached within 5°C of the applicable temperature.
Material should be quenched from the solution heat-treating temperature as rapidly as possible and with minimum delay after removal from the furnace. Quenching is typically performed by immersion of wrought products in a cold water bath, although some forgings are quenched in hot-water. Quenching may be performed by alternative means such as total immersion in an aqueous polymer solution, liquefied gas, hot water, or boiling water, or by air blast or fog to minimize distortion provided samples from the material. The use of high-velocity high-volume jets of cold water is also effective for some materials.
For flat sheet
Temper T3: Solution heat treated at 495°C, quenched, naturally aged. Cold work subsequent to solution heat treatment is required to attain the specified mechanical properties for this temper.
Temper T361: Solution heat treated at 495°C, quenched, naturally aged. Cold work subsequent to solution heat treatment is required to attain the specified mechanical properties for this temper.
Temper T42: Solution heat treated at 495°C, quenched, naturally aged.
Temper T81: Solution heat treated at 495°C, quenched, precipitation heat treated at 190°C, for 12 hours. Cold work prior to any precipitation heat treatment is required to attain the specified mechanical properties for this temper.
Temper T861: Solution heat treated at 495°C, quenched, precipitation heat treated at 190°C, for 8 hours. Cold work prior to any precipitation heat treatment is required to attain the specified mechanical properties for this temper.
Temper T62: Solution heat treated at 495°C, quenched, precipitation heat treated at 190°C, for 9 hours.
For coiled sheet
Temper T4: Solution heat treated at 495°C, quenched, naturally aged.
Temper T42: Solution heat treated at 495°C, quenched, naturally aged.
Temper T62: Solution heat treated at 495°C, quenched, precipitation heat treated at 190°C, for 9 hours.
For plate
Temper T351: Solution heat treated at 495°C, quenched, naturally aged. Stress-relieved by stretching is required to produce a specified amount of permanent set subsequent to solution heat treatment.
Temper T361: Solution heat treated at 495°C, quenched, naturally aged. Cold work subsequent to solution heat treatment is required to attain the specified mechanical properties for this temper.
Temper T42: Solution heat treated at 495°C, quenched, naturally aged.
Temper T851: Solution heat treated at 495°C, quenched, precipitation heat treated at 190°C, for 12 hours. Stress-relieved by stretching is required to produce a specified amount of permanent set prior to any precipitation heat treatment.
Temper T861: Solution heat treated at 495°C, quenched, precipitation heat treated at 190°C, for 8 hours. Cold work prior to any precipitation heat treatment is required to attain the specified mechanical properties for this temper.
Temper T62: Solution heat treated at 495°C, quenched, precipitation heat treated at 190°C, for 9 hours.
AA Alclad 2024 Mechanische Eigenschaften
Temperatur
Benötigen Sie vollständige mechanische Eigenschaften, um die richtige Wahl zu treffen?
Erhalten Sie vollständige Daten zu Festigkeit, Härte, Ermüdung und mehr.
Kostenlose Registrierung erforderlich • Sofortiger Zugriff
AA Alclad 2024 Internationale Werkstoffäquivalente
Anzeige von 6 von 6 Ergebnissen.
Die Äquivalenzkategorien basieren auf dem Vergleich der chemischen Zusammensetzung und der mechanischen Eigenschaften – prüfen Sie stets die Eignung anhand der für Ihre Anwendung geltenden Spezifikation.
Benötigen Sie die vollständige Liste der 6 internationalen Äquivalente?
Sehen Sie alle 6 äquivalenten Werkstoffgüten mit detaillierter Zuordnung nach Norm, Hersteller und Äquivalenzkategorie.
Kostenlose Registrierung erforderlich • Sofortiger Zugriff
Optimieren Sie die Materialauswahl für Ihre Anwendung - Demo vereinbaren
- 6Querverweise
- -Zusammensetzung
- 134Mechanische Eigenschaften
- 20Physikalische Eigenschaften
- 1Wärmebehandlung
- -Metallographie
- -Zerspanbarkeit
- 126Spannung-Dehnung
- -Umformbarkeit
- 6Ermüdung
- -Fraktur
- -Schleicher
- 377Verbindungen
- -Beschichtungen
- -Abmessungen
- -Tribologie
- 1Korrosion
- 38Alterung
- -Witterungsbeständigkeit
- -Bestrahlung
- 3Gesamtzahl der Lieferanten