Ni-P101HT (Germany / DIN) Material Properties
Material group:
Nonferrous Alloys / Nickel / Nickel Alloys
Country/Standard:
Germany / DIN
Data updates
Latest Update: 2020-06
Total number of updates: 2
Update History:
2019-06
Mechanical Properties
Temperature
Physical Properties
Temperature
Composition
CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
Al
VALUE
1.2 – 1.6
UNIT
%
CAS NUMBER
7429-90-5
CRITERIA
B
VALUE
0.003 – 0.010
UNIT
%
CAS NUMBER
7440-42-8
CRITERIA
C
VALUE
0.02 – 0.10
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Ca
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7440-70-2
CRITERIA
Co
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7440-48-4
CRITERIA
Cr
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Cu
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7440-50-8
CRITERIA
Fe
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7439-89-6
CRITERIA
Mg
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7439-95-4
CRITERIA
Mn
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Mo
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7439-98-7
CRITERIA
Ni
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7440-02-0
CRITERIA
P
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7440-21-3
CRITERIA
Ti
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7440-32-6
CRITERIA
Zr
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7440-67-7
EN 3220: 2019 / Aerospace series - Heat resisting nickel base alloy (Ni-P101HT) - Cold worked and softened - Bar and wire for continuous forging or extrusion for fasteners - 3 mm ≤ D ≤ 30 mm
Heat Treatments
- <b>Delivery condition:</b> <br> 10% ≤ cold worked ≤ 30% <br> reduction temperature θ ≤ 870°C <br> <b>Heat treatment:</b> <br> Solution treated 1010°C ≤ θ ≤ 1080°C/1 h/AC, equivalent or faster <br> <b>Use condition:</b> <br>Solution treated stabilised and precipitation treated <br> <b>Heat treatment:</b> <br> Delivery condition <br> + 850°C /4 h /AC, equivalent or faster <br> + 760°C /16 h /AC, equivalent or faster
- Solution treated stabilised and precipitation treated<br> 1010 °C ≤ θ ≤ 1080 °C/t = 1 h/OQ, equivalent or faster<br> + 850 °C/t = 4 h/AC, equivalent or faster<br> + 760 °C/t = 16 h/AC, equivalent or faster
-
19 Cross References
-
34 Composition
-
13 Mechanical Properties
-
3 Physical Properties
-
2 Heat Treatment
-
- Metallography
-
- Machinability
-
- Stress-Strain
-
- Formability
-
- Fatigue
-
- Fracture
-
- Creep
-
- Joints
-
- Coatings
-
- Dimensions
-
- Tribology
-
- Corrosion
-
- Ageing
-
- Weatherability
-
- Irradiation
-
- Total Suppliers