G-AS7GT (Italy / UNI) Material Properties

Material group: Nonferrous Alloys / Aluminium
Country/Standard: Italy / UNI

Data updates

Latest Update: 2016-06
Total number of updates: 1
Update History:

Mechanical Properties


Temperature

0 - 30°C
PROPERTY / VALUE
Yield Strength, Rp0.2 val1
Full data access requires a free trial. Sign Up Free
MPa
view details
Tensile Strength 215 MPa view details
Elongation, A 1.5 % view details
Brinell Hardness (HB) 70 view details
Yield Strength, Rp0.2 val1
Full data access requires a free trial. Sign Up Free
ksi
view details
Tensile Strength 31.2 ksi view details
Elongation, A 1.5 % view details
Brinell Hardness (HB) 70 view details

Physical Properties


Temperature

0 - 30°C
30 - 100°C
100 - 300°C
≥ 300°C
PROPERTY / VALUE
Modulus of Elasticity 69 — 79 GPa view details
Density val1
Full data access requires a free trial. Sign Up Free
kg/dm³
view details
Poisson Coefficient val1
Full data access requires a free trial. Sign Up Free
view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°C
view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°C
view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°C
view details
Thermal Conductivity 155 W/(m∙°C) view details
Heat Capacity val1
Full data access requires a free trial. Sign Up Free
J/(kg∙°C)
view details
Heat Capacity val1
Full data access requires a free trial. Sign Up Free
J/(kg∙°C)
view details
Electrical Resistivity 0.048 Ω∙mm²/m view details
Electrical Conductivity val1
Full data access requires a free trial. Sign Up Free
S/m
view details
Modulus of Elasticity 10 E+03 — 11.5 E+03 ksi view details
Density val1
Full data access requires a free trial. Sign Up Free
lb/in³
view details
Poisson Coefficient val1
Full data access requires a free trial. Sign Up Free
view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°F
view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°F
view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°F
view details
Thermal Conductivity 89.6 BTU/(h∙ft∙°F) view details
Heat Capacity val1
Full data access requires a free trial. Sign Up Free
BTU/(lb∙°F)
view details
Heat Capacity val1
Full data access requires a free trial. Sign Up Free
BTU/(lb∙°F)
view details
Electrical Resistivity 79.8 E-06 Ω∙circular·mil/ft view details
Electrical Conductivity val1
Full data access requires a free trial. Sign Up Free
S/in
view details

Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
Al
VALUE
Remainder
UNIT
%
CAS NUMBER
7429-90-5
CRITERIA
Cu
VALUE
≤ 0.10
UNIT
%
CAS NUMBER
7440-50-8
CRITERIA
Fe
VALUE
≤ 0.20
UNIT
%
CAS NUMBER
7439-89-6
CRITERIA
Mg
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7439-95-4
CRITERIA
Mn
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Ni
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-02-0
CRITERIA
Other each
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
CRITERIA
Other total
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
CRITERIA
Si
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-21-3
CRITERIA
Ti
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-32-6
CRITERIA
Zn
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-66-6

UNI 8024: 1979 / Casting aluminium alloys, Aluminium- silicon-magnesium-titanium alloy (Si 7%, Mg, Ti)

Heat Treatments

  • Solution heat treated and artificially aged (TA1) - Hardening in water 10 to 20°C, after heating 525 to 535°C for at least 9h artificial aging 155 to 165°C for at least 2h and subsequent cooling in still air. <br />Solution heat treated and artificially aged (TA2) - Hardening in water 10 to 20°C, after heating 525 to 535°C for at least 3h artificial aging 155 to 165°C for at least 6 h and subsequent cooling in still air.