Mechanical Properties


Temperature

≤ 0°C
0 - 30°C
PROPERTY / VALUE
Yield Strength, Rp0.2 450 MPa view details
Tensile Strength 690 MPa view details
Elongation, A 25 % view details
Impact Energy val1
Full data access requires a free trial. Sign Up Free
J
view details
Yield Strength, Rp0.2 65.3 ksi view details
Tensile Strength 100.1 ksi view details
Elongation, A 25 % view details
Impact Energy val1
Full data access requires a free trial. Sign Up Free
ft·lb
view details

Physical Properties


Since direct data is not available in the original source, register for a free trial to explore similar or equivalent materials having these properties.

Register Now

Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
≤ 0.030
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
24.0 – 26.0
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Cu
VALUE
0.50 – 1.00
UNIT
%
CAS NUMBER
7440-50-8
CRITERIA
Mn
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Mo
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7439-98-7
CRITERIA
N
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7727-37-9; 17778-88-0
CRITERIA
Ni
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-02-0
CRITERIA
P
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-21-3
CRITERIA
W
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-33-7

A995/A995M: 2020 / Standard Specification for Castings, Austenitic-Ferritic (Duplex) Stainless Steel, for Pressure-Containing Parts

Heat Treatments

  • Heat to 1100°C (2010°F) minimum, hold for sufficient time to heat casting uniformly to temperature, quench in water or rapid cool by other means, or the casting may be furnace cooled to a temperature no lower than 1050°C (1925°F) hold for 15 min minimum, and then quench in water or rapid cool by other means.