ASTM A 356 Grade 9 Cast steels

Material group: Ferrous Alloys / Cast steels
Country/Standard: United States / ASTM

Data updates

Latest Update: 2021-02
Total number of updates: 1
Update History

This material has 118 properties — only a subset is shown here.

Unlock full material properties, including detailed values across temperatures and conditions.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

ASTM A 356 Grade 9 Chemical Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
≤ 0.20
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
1.00 – 1.50
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Mn
VALUE
0.50 – 0.90
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Mo
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7439-98-7
CRITERIA
P
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7440-21-3
CRITERIA
V
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7440-62-2

A356/A356M: 2021 / Steel Castings, Carbon, Low Alloy, and Stainless Steel, Heavy-Walled for Steam Turbines

Looking for full material performance data?

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

This material has 118 properties — only a subset is shown here.

Unlock detailed physical values across temperatures and conditions.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

ASTM A 356 Grade 9 Heat Treatments

  • Heat treatment for mechanical properties:
    Normalizing: The castings shall be heated to and held at the proper temperature for a sufficient time to effect the desired transformation and withdrawn from the furnace and allowed to cool to effect complete transformation.
    Tempering: The casting shall be heated to and held at the proper temperature, which shall be below the transformation range, and then cooled under suitable conditions. The tempering temperature shall not be less than 595°C (1100°F).
    Stress relieving: The stress relieving operation shall be carried out in the same manner as tempering. The temperature shall be within 28°C (50°F), but not exceeding the final tempering temperature.
    Minimum preheat temperature: 150°C (300°F) for t > 13 mm, 10°C (50°F) for t ≤ 13 mm.

ASTM A 356 Grade 9 Mechanical Properties


Temperature

PROPERTY / VALUE
Yield Strength, Rp0.2
415 MPa
Unlock full details
Full data available with free access View Complete Material Data
Tensile Strength
585 MPa
Unlock full details
Full data available with free access View Complete Material Data
Elongation, A
15 %
Unlock full details
Full data available with free access View Complete Material Data
Reduction of Area
val1
Full data available with free access View Complete Material Data
%
Unlock full details
Full data available with free access View Complete Material Data

Need complete mechanical properties to make the right choice?

Get complete data on strength, hardness, fatigue, and more.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

Book A Demo

Optimize material selection for your application - Book a Demo

  • 53 Cross References

  • 8 Composition
  • 4 Mechanical Properties
  • - Physical Properties
  • 1 Heat Treatment
  • - Metallography
  • - Machinability

  • - Stress-Strain
  • - Formability
  • - Fatigue
  • - Fracture
  • 3 Creep

  • 7 Joints
  • - Coatings
  • - Dimensions
  • - Tribology

  • - Corrosion
  • - Ageing
  • - Weatherability
  • - Irradiation

  • 42 Total Suppliers